410 Ryðfrítt stál vörur

Mar 23, 2026

Skildu eftir skilaboð

UNS S30908 Stainless Steel – High-Chromium Heat-Resistant Utility Alloy304L Stainless Steel Sheet for Chemical Tank Linings304L Stainless Steel Coil for Petrochemical Pipelines

Efnasamsetningar

Frumefni

C

Mn

Si

Kr

Ni

P

S

Fe

Samsetningarsvið (%) 0.08 – 0.15 1.00 hámark 1.00 hámark 11.50 – 13.50 0,75 hámark 0,04 hámark 0,03 hámark Jafnvægi

Vélrænir eiginleikar

Vélræn eign

Gildi (mæling)

Gildi (Imperial)

Togstyrkur 480 – 620 MPa 70 – 90 ksi
Afkastastyrkur 275 – 450 MPa 40 – 65 ksi
Brinell hörku (HB) 170 – 201 HB 170 – 201 HB
Rockwell hörku (HRC) 20 – 30 HRC 20 – 30 HRC
Vickers hörku (HV) 180 – 230 HV 180 – 230 HV
Lenging 20% – 25% 20% – 25%
Teygjustuðull 200 GPa 29 x 10³ ksi