316L ryðfrítt stálplata 1,0 mm kaldvalsað ASTM A240 DIN1.4404

Mar 23, 2026

Skildu eftir skilaboð

What is 1.4537 Stainless Steel?What is 1.4529 Stainless Steel?Stainless Steel - Grade 440 (UNS S44000)

Tegund Ryðfrítt stálplata
Einkunn 200 Ritröð:201/202
300 Röð:301/302/303/304/304 L/304 N/309/309 S/310/316/316 L/321/347
400 röð: 403/408/409/410/416/420/430/431/440/440A/440B/440C/439/443/444
600 Röð: 610/620/630
900 röð: 904L
Þykkt 0,3-100 mm
Breidd 600mm, 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm osfrv
Lengd 2000mm, 2440mm, 3000mm, 5800mm, 6000mm osfrv
Yfirborð BA/2B/NO.1/NO.4/8K/HL
Gæðapróf við getum boðið MTC, ISO, SGS, BV osfrv
Greiðsluskilmálar L/CT/T (30% INNborgun)
Stock eða ekki Nóg af lager
Sýnishorn Ókeypis sýnishorn
Umsókn Efnaiðnaður, lækningatæki, byggingarefni, skreytingar,
Eldhúsvörur, matur osfrv
Afhendingartími Innan 7-15 daga

 

 

Samsvarandi einkunnir af A240 ryðfríu stáli 316L blöðum og plötum

STANDAÐUR WERKSTOFF NR. JIS BS GOST AFNOR EN
SS 316L 1.4404/1.4435 S31603 SUS 316L 316S11/316S13 03Ch17N14M3 / 03Ch17N14M2 Z3CND17-11-02 / Z3CND18-14-03 X2CrNiMo17-12-2 / X2CrNiMo18-14-3

Ryðfrítt stál 316L blöð og plötur Efnafræðilegir eiginleikar

Einkunn C Mn Si P S Kr Mo Ni N
SS 316L 0,035 hámark 2,0 hámark 1.00 hámark 0,045 hámark 0,030 hámark 16 – 18 2 – 3 10 – 14 68,89 mín

SS 316L blöð og plötur Vélrænir eiginleikar

Þéttleiki Bræðslumark Togstyrkur Afrakstursstyrkur (0,2% offset) Lenging
8,0 g/cm3 1399 gráður (2550 gráður F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 35 %

Hringdu í okkur